CNS-SCH23
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Mo (%) | Vloeigrens (Mpa) | Treksterkte (Mpa) | Rekbaarheid (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.2-0.6 | Si(%)(%) ≦2.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 18.0-22.0 | Cr (%)(%) 28.0-32.0 | Mo (%)(%) ≦0,5 | Vloeigrens (Mpa)(%) ≧245 | Treksterkte (Mpa)(%) ≧450 | Rekbaarheid (%)(%) ≧8 |
Toepassingen
- Hittestand staal gietstukken
Landcode
- CNS
Standaard
- 4002
Staaltype
- SCH23
Gerelateerd Staaltype
Staaltype | Standaard | Landcode | Meer | SCH23 | 4002 | CNS | Meer | ZG40Cr30-Ni20 | 8492 | GB | Meer | SCH23 | G5122 | JIS | Meer | HL | A297 | ASTM | Meer |
---|