C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Cu (%) | Al(%) | Ti (%) | Vloeigrens (Mpa) | Treksterkte (Mpa) | Rekbaarheid (%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.05 | Si(%)(%) ≦0,5 | Mn(%)(%) ≦1.0 | P(%)(%) ≦0.03 | S(%)(%) ≦0.015 | Ni (%)(%) 38,0-46,0 | Cr (%)(%) 19,5-23,5 | Cu (%)(%) 1.5-3.0 | Al(%)(%) ≦0.2 | Ti (%)(%) 0.6-1.2 | Vloeigrens (Mpa)(%) ≧235 | Treksterkte (Mpa)(%) ≧580 | Rekbaarheid (%)(%) ≧30 |
Toepassingen
- Corrosiebestendige en hittebestendige superlegering platen en staven
Overig
- Mo : 2.5-3.5
Landcode
- JIS
Staaltype
- NCF825
Gerelateerd Staaltype
Staaltype | Landcode | Meer | NCF825 | CNS | Meer | NCF825 | JIS | Meer |
---|