ASTM-Classe 3
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Mo (%) | V(%) | Cu (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.45 | Si(%)(%) 0,15-0,35 | Mn(%)(%) 0,4-0,9 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) ≦0,5 | Cr (%)(%) ≦1,25 | Mo (%)(%) ≧0,15 | V(%)(%) ≦0,5 | Cu (%)(%) ≦0,35 | Contrainte de rendement (Mpa)(%) ≧550 | Contrainte de traction (Mpa)(%) ≧725 | Allongement (%)(%) ≧19 |
Applications
- Forgés en acier au chrome-molybdène pour usage général
Code pays
- ASTM
Norme
- A291
Type d'acier
- Class 3
Type d'acier associé
Type d'acier | Norme | Code pays | Suite | SFCM75 | 4041 | CNS | Suite | SFCM740 | G3221 | JIS | Suite | Gr.E | A290 | ASTM | Suite | Gr.F | A290 | ASTM | Suite | Class 3 | A291 | ASTM | Suite |
---|