CNS-SCH24
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Mo (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0,35-0,75 | Si(%)(%) ≦2,0 | Mn(%)(%) ≦2,0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 33,0-37,0 | Cr (%)(%) 24,0-28,0 | Mo (%)(%) ≦0,5 | Contrainte de rendement (Mpa)(%) ≧235 | Contrainte de traction (Mpa)(%) ≧440 | Allongement (%)(%) ≧5 |
Applications
- Fonderies d'acier résistant à la chaleur
Code pays
- CNS
Norme
- 4002
Type d'acier
- SCH24
Type d'acier associé
Type d'acier | Norme | Code pays | Suite | SCH24 | 4002 | CNS | Suite | ZG45Ni35-Cr26 | 8492 | GB | Suite | SCH24 | G5122 | JIS | Suite | HP | A297 | ASTM | Suite | G-X40Ni-CrSi35-2-5 | 17465 | DIN | Suite |
---|