CNS-SCMnH11
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
---|---|---|---|---|---|---|---|---|
C(%)(%) 0.9-1.3 | Si(%)(%) ≦0,8 | Mn(%)(%) 11,0-14,0 | P(%)(%) ≦0,07 | S(%)(%) ≦0.04 | Cr (%)(%) 1.5-2.5 | Contrainte de rendement (Mpa)(%) ≧390 | Contrainte de traction (Mpa)(%) ≧740 | Allongement (%)(%) ≧20 |
Applications
- Fonte en acier à haute teneur en manganèse
Code pays
- CNS
Norme
- 3830
Type d'acier
- SCMnH11
Type d'acier associé
Type d'acier | Norme | Code pays | Suite | SCMnH11 | 3830 | CNS | Suite | SCMnH21 | 3830 | CNS | Suite | ZGMn13-4(GB) | GB | Suite | SCMnH11 | G5131 | JIS | Suite | SCMnH21 | G5131 | JIS | Suite | C | A128 | ASTM | Suite | GX120-Mn12 | 17145 | DIN | Suite |
---|