CNS-SCS17
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0,2 | Si(%)(%) ≦0,2 | Mn(%)(%) ≦0,2 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 12,0-15,0 | Cr (%)(%) 22,0-26,0 | Contrainte de rendement (Mpa)(%) ≧205 | Contrainte de traction (Mpa)(%) ≧480 | Allongement (%)(%) ≧28 |
Applications
- Fonderies en acier inoxydable
Code pays
- CNS
Norme
- 4000
Type d'acier
- SCS17
Type d'acier associé
Type d'acier | Norme | Code pays | Suite | CH-20 | A473 | ASTM | Suite | SCS17 | G5121 | JIS | Suite | CH-20 | A351 | ASTM | Suite | SCS17 | 4000 | CNS | Suite |
---|