CNS-SCS4
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0,15 | Si(%)(%) ≦1.5 | Mn(%)(%) ≦1.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 1.5-2.5 | Cr (%)(%) 11.5-14.0 | Contrainte de rendement (Mpa)(%) ≧490 | Contrainte de traction (Mpa)(%) ≧640 | Allongement (%)(%) ≧13 |
Applications
- Fonderies en acier inoxydable
Code pays
- CNS
Norme
- 4000
Type d'acier
- SCS4
Type d'acier associé
Type d'acier | Norme | Code pays | Suite | SCS4 | 4000 | CNS | Suite | SCS4 | G5121 | JIS | Suite |
---|