CNS-SCS6
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Mo (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0,06 | Si(%)(%) ≦1.0 | Mn(%)(%) ≦1.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0,03 | Ni (%)(%) 3.5-4.5 | Cr (%)(%) 11.5-14.0 | Mo (%)(%) 0.4-1.0 | Contrainte de rendement (Mpa)(%) ≧550 | Contrainte de traction (Mpa)(%) ≧750 | Allongement (%)(%) ≧15 |
Applications
- Fonderies en acier inoxydable
Code pays
- CNS
Norme
- 4000
Type d'acier
- SCS6
Type d'acier associé
Type d'acier | Norme | Code pays | Suite | SCS6 | 4000 | CNS | Suite | SCS6 | G5121 | JIS | Suite | CA-6NM | A743 | ASTM | Suite |
---|