GB-ZG40Cr30-Ni20
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Mo (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.2-0.6 | Si(%)(%) ≦2,0 | Mn(%)(%) ≦2,0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 18,0-22,0 | Cr (%)(%) 28,0-32,0 | Mo (%)(%) ≦0,5 | Contrainte de rendement (Mpa)(%) ≧245 | Contrainte de traction (Mpa)(%) ≧450 | Allongement (%)(%) ≦8 |
Applications
- Fonderies d'acier résistant à la chaleur
Code pays
- GB
Norme
- 8492
Type d'acier
- ZG40Cr30-Ni20
Type d'acier associé
Type d'acier | Norme | Code pays | Suite |
SCH23 |
4002 | CNS | Suite |
ZG40Cr30-Ni20 |
8492 | GB | Suite |
SCH23 |
G5122 | JIS | Suite |
HL |
A297 | ASTM | Suite |
---|