JIS-SCH18
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Mo (%) | Contrainte de rendement (Mpa) | Contrainte de traction (Mpa) | Allongement (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.2-0.5 | Si(%)(%) ≦2,0 | Mn(%)(%) ≦2,0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 14.0-18.0 | Cr (%)(%) 26.0-30.0 | Mo (%)(%) ≦0,5 | Contrainte de rendement (Mpa)(%) ≧235 | Contrainte de traction (Mpa)(%) ≧490 | Allongement (%)(%) ≧8 |
Applications
- Fonderies d'acier résistant à la chaleur
Code pays
- JIS
Norme
- G5122
Type d'acier
- SCH18
Type d'acier associé
Type d'acier | Norme | Code pays | Suite | SCH18 | 4002 | CNS | Suite | ZG40Cr28-Ni16 | 8492 | GB | Suite | SCH18 | G5122 | JIS | Suite | HI | A297 | ASTM | Suite |
---|