C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Mo (%) | Vloeigrens (Mpa) | Treksterkte (Mpa) | Rekbaarheid (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.2-0.5 | Si(%)(%) ≦2.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni (%)(%) 8.0-11.0 | Cr (%)(%) 26.0-30.0 | Mo (%)(%) ≦0,5 | Vloeigrens (Mpa)(%) ≧275 | Treksterkte (Mpa)(%) ≧540 | Rekbaarheid (%)(%) ≧5 |