CNS-SCH17
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | Tegangan Hasil (Mpa) | Tegangan Tarik (Mpa) | Pemanjangan (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.2-0.5 | Si(%)(%) ≦2.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) 8.0-11.0 | Cr(%)(%) 26.0-30.0 | Mo(%)(%) ≦0.5 | Tegangan Hasil (Mpa)(%) ≧275 | Tegangan Tarik (Mpa)(%) ≧540 | Pemanjangan (%)(%) ≧5 |
Aplikasi
- Tuangan Keluli Tahan Panas
Kod Negara
- CNS
Standard
- 4002
Jenis Baja
- SCH17
Jenis Baja yang Berkaitan
Jenis Baja | Standard | Kod Negara | More | SCH17 | 4002 | CNS | More | SCH17 | G5122 | JIS | More | HE | A297 | ASTM | More |
---|