ASTM-F321
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Ti(%) | Yield stress (Mpa) | Tensile stress (Mpa) | Elongation (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.08 | Si(%)(%) ≦1.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.045 | S(%)(%) ≦0.03 | Ni(%)(%) 9.0-12.0 | Cr(%)(%) ≧17.0 | Ti(%)(%) 5xC%-0.7 | Yield stress (Mpa)(%) ≧205 | Tensile stress (Mpa)(%) ≧515 | Elongation (%)(%) ≧30 |
Applications
- Forged Stainless Steel Flanges/Fittings/Valves and Part of Pressure Vessels for High
Country Code
- ASTM
Standard
- A182
Steel Type
- F321
Relate Steel Type
Steel Type | Standard | Country Code | More |
F321 |
8702 | CNS | More |
SUSF321 |
G3214 | JIS | More |
F321 |
A182 | ASTM | More |
F321 |
A336 | ASTM | More |
---|