ASTM-W1-7
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | W(%) | V(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.7-0.8 | Si(%)(%) 0.1-0.4 | Mn(%)(%) 0.1-0.4 | P(%)(%) ≦0.025 | S(%)(%) ≦0.025 | Ni(%)(%) ≦0.2 | Cr(%)(%) ≦0.15 | Mo(%)(%) ≦0.1 | W(%)(%) ≦0.15 | V(%)(%) ≦0.1 | Cu(%)(%) ≦0.2 |
Applications
- Carbon Tool Steels
Other
- Annealing HB : ≦202
- Quenching HRC : ≧64
Country Code
- ASTM
Steel Type
- W1-7
Relate Steel Type
Steel Type | Country Code | More |
T7A |
GB | More |
W1-7 |
ASTM | More |
C70W1 |
DIN | More |
C70W2 |
DIN | More |
SK7 |
CNS | More |
T7 |
GB | More |
SK7 |
JIS | More |
---|