CNS-SCH22
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | Yield stress (Mpa) | Tensile stress (Mpa) | Elongation (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.35-0.45 | Si(%)(%) ≦1.75 | Mn(%)(%) ≦1.5 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) 19.0-22.0 | Cr(%)(%) 23.0-27.0 | Mo(%)(%) ≦0.5 | Yield stress (Mpa)(%) ≧235 | Tensile stress (Mpa)(%) ≧440 | Elongation (%)(%) ≧8 |
Applications
- Heat Resisting Steel Castings
Country Code
- CNS
Standard
- 4002
Steel Type
- SCH22
Relate Steel Type
Steel Type | Standard | Country Code | More | SCH22 | 4002 | CNS | More | ZG40Cr25-Ni20 | 8492 | GB | More | SCH22 | G5122 | JIS | More | HK40 | A351 | ASTM | More | G-X40Cr-NiSi25-20 | 17465 | DIN | More |
---|