CNS-SCS12
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Yield stress (Mpa) | Tensile stress (Mpa) | Elongation (%) |
---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.2 | Si(%)(%) ≦2.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) 8.0-11.0 | Cr(%)(%) 18.0-20.0 | Yield stress (Mpa)(%) ≧205 | Tensile stress (Mpa)(%) ≧480 | Elongation (%)(%) ≧28 |
Applications
- Stainless Steel Castings
Country Code
- CNS
Standard
- 4000
Steel Type
- SCS12
Relate Steel Type
Steel Type | Standard | Country Code | More | SCS12 | 4000 | CNS | More | ZG1Cr-18Ni9 | 2100 | GB | More | SCS12 | G5121 | JIS | More | CF-20 | A743 | ASTM | More | G-X10Cr-Nil8-8 | 17445 | DIN | More |
---|