JIS-SCCrM3B
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | Yield stress (Mpa) | Tensile stress (Mpa) | Elongation (%) |
---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.3-0.4 | Si(%)(%) 0.3-0.6 | Mn(%)(%) 0.5-0.8 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Cr(%)(%) 0.8-1.2 | Mo(%)(%) 0.15-0.35 | Yield stress (Mpa)(%) ≧540 | Tensile stress (Mpa)(%) ≧740 | Elongation (%)(%) ≧9 |
Applications
- High Tensile Strength Carbon Steel Castings and Low Alloy Steel Castings for Structur
Country Code
- JIS
Standard
- G5111
Steel Type
- SCCrM3B
Relate Steel Type
Steel Type | Standard | Country Code | More | SCCrM3B | 7145 | CNS | More | SCCrM3B | G5111 | JIS | More | 105-85 | A148 | ASTM | More |
---|