JIS-SPA-C
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Cu(%) | Thick (mm) | Yield stress (Mpa) | Tensile stress (Mpa) | Elongation (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.12 | Si(%)(%) 0.25-0.75 | Mn(%)(%) 0.20-0.50 | P(%)(%) 0.07-0.15 | S(%)(%) ≦0.04 | Cr(%)(%) 0.30-1.25 | Cu(%)(%) 0.25-0.60 | Thick (mm)(%) ≦6.0 | Yield stress (Mpa)(%) ≧315 | Tensile stress (Mpa)(%) ≧450 | Elongation (%)(%) ≧26 |
Applications
- Superior Atmospheric Corrosion Resisting Rolled Steels
Country Code
- JIS
Standard
- G3125
Steel Type
- SPA-C
Relate Steel Type
Steel Type | Standard | Country Code | More | SPA-C | 4620 | CNS | More | SPA-C | G3125 | JIS | More |
---|