C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | W(%) | Cu(%) | Tegangan Hasil (Mpa) | Tegangan Tarik (Mpa) | Pemanjangan (%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.2 | Si(%)(%) ≦0.75 | Mn(%)(%) 0.5-0.8 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) ≦0.5 | Cr(%)(%) 4.0-6.5 | Mo(%)(%) 0.45-0.65 | W(%)(%) ≦0.1 | Cu(%)(%) ≦0.5 | Tegangan Hasil (Mpa)(%) ≧410 | Tegangan Tarik (Mpa)(%) ≧620 | Pemanjangan (%)(%) ≧17 |
Aplikasi
- Tuangan Keluli untuk Perkhidmatan Suhu Tinggi dan Tekanan Tinggi
Kod Negara
- CNS
Standard
- 7147
Jenis Baja
- SCPH61
Jenis Baja yang Berkaitan
Jenis Baja | Standard | Kod Negara | More |
Gr.WC5 |
A217 | ASTM | More |
SCPH61 |
G5151 | JIS | More |
SCPH61 |
7147 | CNS | More |
---|