CNS-SCS16A
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | Tegangan Hasil (Mpa) | Tegangan Tarik (Mpa) | Pemanjangan (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.03 | Si(%)(%) ≦1.5 | Mn(%)(%) ≦1.5 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) 9.0-13.0 | Cr(%)(%) 17.0-21.0 | Mo(%)(%) 2.0-3.0 | Tegangan Hasil (Mpa)(%) ≧205 | Tegangan Tarik (Mpa)(%) ≧480 | Pemanjangan (%)(%) ≧23 |
Aplikasi
- Tuangan Keluli Tahan Karat
Kod Negara
- CNS
Standard
- 4000
Jenis Baja
- SCS16A
Jenis Baja yang Berkaitan
Jenis Baja | Standard | Kod Negara | More | SCS16A | 4000 | CNS | More | SCS16A | G5121 | JIS | More | CF-3M | A351 A743 A744 | ASTM | More |
---|