CNS-SPA-H
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Cu(%) | Tebal (mm) | Tegangan Hasil (Mpa) | Tegangan Tarik (Mpa) | Pemanjangan (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.12 | Si(%)(%) 0.25-0.75 | Mn(%)(%) 0.20-0.50 | P(%)(%) 0.07-0.15 | S(%)(%) ≦0.04 | Cr(%)(%) 0.30-1.25 | Cu(%)(%) 0.25-0.60 | Tebal (mm)(%) ≦6.0 | Tegangan Hasil (Mpa)(%) ≧345 | Tegangan Tarik (Mpa)(%) ≧480 | Pemanjangan (%)(%) ≧22 |
Aplikasi
- Keluli Gulung Tahan Karat Atmosfera Superior
Kod Negara
- CNS
Standard
- 4620
Jenis Baja
- SPA-H
Jenis Baja yang Berkaitan
Jenis Baja | Standard | Kod Negara | More | SPA-H | 4620 | CNS | More | SPA-H | G3125 | JIS | More | Type1 | A242 | ASTM | More |
---|