CNS-NCF751
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni (%) | Cr (%) | Cu (%) | Al(%) | Ti (%) | Fe (%) | Dikte (mm) | Vloeigrens (Mpa) | Treksterkte (Mpa) | Rekbaarheid (%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.1 | Si(%)(%) ≦0,5 | Mn(%)(%) ≦1.0 | P(%)(%) ≦0.03 | S(%)(%) ≦0.015 | Ni (%)(%) ≧70.0 | Cr (%)(%) 14.0-17.0 | Cu (%)(%) ≦0,5 | Al(%)(%) 0,9-1,5 | Ti (%)(%) 2.0-2.6 | Fe (%)(%) 5.0-9.0 | Dikte (mm)(%) -≦100 | Vloeigrens (Mpa)(%) ≧615 | Treksterkte (Mpa)(%) ≧960 | Rekbaarheid (%)(%) ≧8 |
Toepassingen
- Corrosiebestendige en hittebestendige superlegering platen en staven
Landcode
- CNS
Staaltype
- NCF751
Gerelateerd Staaltype
Staaltype | Landcode | Meer |
NCF751 |
CNS | Meer |
NCF751 |
JIS | Meer |
---|