CNS-NCF751
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Cu(%) | Al(%) | Ti(%) | Fe(%) | Tebal (mm) | Tegangan Hasil (Mpa) | Tegangan Tarik (Mpa) | Pemanjangan (%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.1 | Si(%)(%) ≦0.5 | Mn(%)(%) ≦1.0 | P(%)(%) ≦0.03 | S(%)(%) ≦0.015 | Ni(%)(%) ≧70.0 | Cr(%)(%) 14.0-17.0 | Cu(%)(%) ≦0.5 | Al(%)(%) 0.9-1.5 | Ti(%)(%) 2.0-2.6 | Fe(%)(%) 5.0-9.0 | Tebal (mm)(%) -≦100 | Tegangan Hasil (Mpa)(%) ≧615 | Tegangan Tarik (Mpa)(%) ≧960 | Pemanjangan (%)(%) ≧8 |
Aplikasi
- Lembaran, Plat dan Bar Superalloy Tahan Karat dan Tahan Panas
Kod Negara
- CNS
Jenis Baja
- NCF751
Jenis Baja yang Berkaitan
Jenis Baja | Kod Negara | More | NCF751 | CNS | More | NCF751 | JIS | More |
---|