CNS-NCF751
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Cu(%) | Al(%) | Ti(%) | Fe(%) | Thick (mm) | Yield stress (Mpa) | Tensile stress (Mpa) | Elongation (%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) ≦0.1 | Si(%)(%) ≦0.5 | Mn(%)(%) ≦1.0 | P(%)(%) ≦0.03 | S(%)(%) ≦0.015 | Ni(%)(%) ≧70.0 | Cr(%)(%) 14.0-17.0 | Cu(%)(%) ≦0.5 | Al(%)(%) 0.9-1.5 | Ti(%)(%) 2.0-2.6 | Fe(%)(%) 5.0-9.0 | Thick (mm)(%) -≦100 | Yield stress (Mpa)(%) ≧615 | Tensile stress (Mpa)(%) ≧960 | Elongation (%)(%) ≧8 |
Applications
- Corrosion-Resisting and Heat-Resisting Superalloy Sheets Plates and Bars
Country Code
- CNS
Steel Type
- NCF751
Relate Steel Type
Steel Type | Country Code | More | NCF751 | CNS | More | NCF751 | JIS | More |
---|