CNS-SCH13
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Ni(%) | Cr(%) | Mo(%) | Yield stress (Mpa) | Tensile stress (Mpa) | Elongation (%) |
---|---|---|---|---|---|---|---|---|---|---|
C(%)(%) 0.2-0.5 | Si(%)(%) ≦2.0 | Mn(%)(%) ≦2.0 | P(%)(%) ≦0.04 | S(%)(%) ≦0.04 | Ni(%)(%) 11.0-14.0 | Cr(%)(%) 24.0-28.0 | Mo(%)(%) ≦0.5 | Yield stress (Mpa)(%) ≧235 | Tensile stress (Mpa)(%) ≧490 | Elongation (%)(%) ≧8 |
Applications
- Heat Resisting Steel Castings
Country Code
- CNS
Standard
- 4002
Steel Type
- SCH13
Relate Steel Type
Steel Type | Standard | Country Code | More | SCH13 | 4002 | CNS | More | SCH13A | 4002 | CNS | More | ZG35Cr26-Ni12 | 8492 | GB | More | SCH13 | G5122 | JIS | More | SCH13A | G5122 | JIS | More | HH | A297 | ASTM | More | G-X40Cr-NiSi22-9 | 17465 | DIN | More |
---|